Brian Preusser says: I would have never guessed the flaming/etching process was like that. Is that a ferric chloride solution? Very cool random vapor jacket patterning, I always thought it was a randomly sprayed oil applied prior to flame treatment. May 3, 2022 at 3:08 PM
I would have never guessed the flaming/etching process was like that. Is that a ferric chloride solution? Very cool random vapor jacket patterning, I always thought it was a randomly sprayed oil applied prior to flame treatment.
Very cool to see the process!